Free shipping over $800Shop now

Guides

Understanding Tile Testing: Five Tests That Measure Performance

•By Caden Tile Team
Understanding Tile Testing: Five Tests That Measure Performance
Image: Aquabella Beachfront Santa Monica 6x6 Porcelain Pool Tile — Caden Tile

Choosing tile involves more than color and style. Laboratory tests help explain how a tile responds to chemicals, freezing temperatures, force, bonding, and stains. Understanding these tests makes product specifications easier to compare.

Who Develops and Performs the Tests?

  • ASTM International publishes test methods. Its ceramic tile standards establish procedures for measuring properties such as breaking strength, chemical resistance, and freeze-thaw resistance. Source: ASTM ceramic standards
  • Testing laboratories perform the measurements. For example, International Product Assurance Laboratories—IPA Laboratories—in Anderson, South Carolina, lists all five testing categories among its ceramic tile services. It offers ASTM, ANSI, and ISO testing, including a broad range of ISO/IEC 17025-accredited tests. Source: IPA Laboratories
  • The supplied reports were issued by the Tile Institute of America, signed by Gerald M. Halweg as president/CEO. That identifies the organization responsible for those particular reports; other laboratories can perform the same test methods.

About the Example Reports

The examples in this article come from five reports the Tile Institute of America issued on November 30, 2023, for AquaBella/Main Street Art, Inc. They share the same product and sampling details:

  • Product: Aquabella Beachfront Series porcelain tile, factory "A-56".
  • Colors and formats tested: Balboa, Crystal Cove, Malibu, Palisades, and Santa Monica, in 6" x 6", 6" x 6" SBN, 3" x 12", and 1" x 2" formats, plus blends.
  • Sampling: New tiles were sent to the laboratory in sealed manufacturer's boxes and selected at random.
  • Requirements cited: Four of the reports compare results with the general requirements of ANSI A137.1, the American national specification for ceramic tile. The stain report states its own pass criteria.

The five Beachfront colors covered by the reports. Images: the Balboa, Crystal Cove, Malibu, Palisades, and Santa Monica product pages on Caden Tile. Click a color to open its page.

1Chemical Resistance — ASTM C650

What it measures: How tile surfaces respond to prolonged contact with chemical substances.

  • How it works: Samples undergo controlled chemical exposure, followed by an assessment of the effect on the surface. Chemical concentration, exposure time, and temperature are important parts of interpreting the result.
  • Why it matters: This test helps evaluate tile for counters, washrooms, and other locations exposed to food, waste substances, or strong cleaning agents. Source: ASTM C650

Video: ASTM C650 - Standard Test Method for Determination of Resistance to Chemical Substances by Hydro Kalon Limited on YouTube.

Procedure in the supplied report

  • Chemicals: 10% hydrochloric acid (an acid) and 10% potassium hydroxide (an alkali).
  • Temperature: Controlled at 75 ± 5°F (24 ± 3°C).
  • Exposure time: 24 hours.

Requirement and result

  • Requirement: ANSI A137.1 — when tested as described in ASTM C650, the tile shall not be affected.
  • Result: Passed. The report states that all listed tile types yielded results compliant with the requirement.

These conditions describe that report's testing and should be checked when comparing results.

Report reference: Aquabella Beachfront chemical resistance report, ASTM C650 (PDF)

2Freeze-Thaw Resistance — ASTM C1026

What it measures: A tile's resistance to repeated freezing and thawing.

  • How it works: Laboratory equipment cycles samples through controlled freezing and thawing conditions. The procedure helps evaluate ceramic and glass tiles intended for outdoor service in freezing climates. Source: ASTM C1026
  • What laboratories look for: The supplied report identifies damage such as cracks, chipping, surface crazing, and spalling—the flaking or breaking away of material.

Video: ASTM C666: Concrete Freeze/Thaw Testing Demonstrated by Master Builders Solutions on YouTube. It shows freeze-thaw cycling on concrete (ASTM C666); the tile method, ASTM C1026, applies the same freeze-and-thaw principle to tile.

Procedure in the supplied report

  • Specimens: Ten tiles.
  • Freezing: Specimens were placed in a freezing chamber and brought to 0°F (-18°C) over 6–8 hours.
  • Thawing: Specimens were then placed in water at 50–60°F (10–16°C) for at least 30 minutes.
  • Cycles: 15 freeze-thaw cycles.
  • Damage recorded: The report uses these codes: Cz = crazing, Ch = chipping, Sp = spalling, Bc = body checks, Cr = cracks.

Requirement and result

  • Requirement: After 15 cycles, the units must show no evidence of failure to the body or surface and no evidence of disintegration.
  • Result: All units passed.

The report's cycle count should not be treated as a universal requirement for every edition of the standard.

Report reference: Aquabella Beachfront freeze-thaw report, ASTM C1026 (PDF)

Why installation matters: Even frost-resistant tile can suffer damage when water enters grout joints or voids in the setting bed. Exterior suitability also depends on drainage, installation methods, and the manufacturer's application rating. Source: TCNA frost-resistance guidance

3Breaking Strength — ASTM C648

What it measures: The force required to break a tile under a specified loading arrangement.

  • How it works: A tile rests on three supports while force is applied at its center until it breaks.
  • How results are expressed: Breaking force is reported in pounds-force or newtons.

Procedure in the supplied report

  • Samples: New tiles from sealed manufacturer's boxes, selected at random from unopened containers.
  • Fixture for larger tiles: Three 3/8" diameter stainless steel balls spaced on a circle 3-15/32" in diameter.
  • Fixture for smaller tiles: Three 1/8" diameter stainless steel balls spaced on a circle 0.645" in diameter.
  • Loading: Force applied at the center of the tile, increasing at 1,000 pounds-force (lbf) per minute until the tile broke.

Requirement and result

  • Requirement: ANSI A137.1 — average breaking strength of at least 90 lbf for glazed wall tile and at least 250 lbf for glazed paver tile.
  • Result: Passed. The report states that all listed tile types exceeded these requirements; it does not list the individual breaking loads.

Report reference: Aquabella Beachfront breaking strength report, ASTM C648 (PDF)

How to read the result: Breaking strength describes performance in this fixture. Assessing an entire floor installation is a separate task; ASTM lists C627 specifically for evaluating ceramic floor tile installation systems. Source: ASTM ceramic standards

4Bond Strength — ASTM C482

What it measures: A tile's ability to develop an adequate bond to Portland cement paste.

  • How it works: Bonded specimens are subjected to force to evaluate the tile bond. Results can be compared with minimum limits appropriate to the expected service conditions.
  • What matters: The location of failure matters. ASTM explains that separation between the bond coat and setting bed—or breakage of the setting bed itself—is not considered failure of the tile bond. Source: ASTM C482

Video: ASTM C482 Bond Strength Test Prep by International Product Assurance Laboratories on YouTube.

Procedure in the supplied report

  • Bonding: Tiles were bonded to concrete units with latex-modified thin-set mortar (the report cites ANSI A118.4, A118.11, and A118.15 mortars).
  • Modification: The report identifies this as a modified procedure, using a latex-modified (resin-enhanced) thin-set bond coat as recommended by industry standards instead of a pure cement bond coat.
  • Curing: 28 days before testing.
  • Loading: Samples were placed on a test fixture and loaded in shear at 1,000 lbf per minute until the bond sheared.

Requirement and result

  • Requirement: ANSI A137.1 — average bond strength of at least 50 pounds per square inch (psi).
  • Other references cited: The report also notes a 50 psi shearing stress under the UBC (Uniform Building Code), and 50 psi plus a 100 psi bond strength for California DSA/SS and OSHPD 1 projects.
  • Result: Passed. The report states that all listed tile types exceeded these requirements; it does not list the individual bond strengths.

Report reference: Aquabella Beachfront bond shear strength report, ASTM C482 (PDF)

Why it matters: When comparing reports, check the bonding material, curing period, and any modifications to the standard procedure.

5Stain Resistance — T-72 and ASTM C1378

What it measures: Whether staining substances leave visible marks after a defined exposure and cleaning process.

Procedure in the supplied T-72 report

  • Staining materials: Six common household materials—cola, lemon juice, mustard, bacon grease, ketchup, and cooking oil.
  • Exposure: For each material, one sample was covered with a Petri dish and one was left uncovered, and both remained for 24 hours.
  • Cleaning: Samples were cleaned with Ajax Industrial Cleaner and water, then examined for remaining surface stains.

Requirement and result

  • Requirement: No evidence of any surface stain remaining, and all traces of the staining materials can be washed from the tile's surface.
  • Result: Pass. No stain remained on either the covered or uncovered samples:
Staining materialUncoveredCovered
ColaNo stainNo stain
Lemon juiceNo stainNo stain
MustardNo stainNo stain
Bacon greaseNo stainNo stain
KetchupNo stainNo stain
Cooking oilNo stainNo stain

Report reference: Aquabella Beachfront stain resistance report, T-72 (PDF)

Another standardized method: ASTM C1378 evaluates staining resistance using specified agents, including inks and colored solutions. After exposure, samples are cleaned in a defined manner and visually inspected. It is a separate method from the T-72 procedure described above. Source: ASTM C1378

The Five Tests at a Glance

TestConditions in the supplied reportRequirement citedResult
Chemical resistance (ASTM C650)10% hydrochloric acid and 10% potassium hydroxide, 24 hours at 75 ± 5°FTile not affectedPassed
Freeze-thaw (ASTM C1026)10 specimens, 15 cycles, frozen to 0°F and thawed in 50–60°F waterNo body or surface failure, no disintegrationPassed
Breaking strength (ASTM C648)Three-point support, center load at 1,000 lbf per minute90 lbf (glazed wall tile), 250 lbf (glazed paver tile)Passed
Bond strength (ASTM C482, modified)Latex-modified thin-set on concrete, 28-day cure, shear load at 1,000 lbf per minute50 psi averagePassed
Stain resistance (T-72)Six household materials, covered and uncovered, 24 hours, cleaned with Ajax and waterNo surface stain remainingPassed

What to Look for in a Tile Test Report

A useful report should clearly identify:

  • The product and samples tested.
  • The test method and edition, including modifications.
  • Exposure conditions, materials, and curing times.
  • Measured results and acceptance criteria.
  • The laboratory responsible for the testing.

These details give a "pass" result meaning and help you judge whether the tested conditions match your project.